Agrinol EТ-2U, Agrinol RG, Agrinol EHP, Agrinol HP |
Agrinol EТ-2UТУ У 23.2-30802090-005-2003Emulsifier Agrinol ET-2U is a concentrated product of oil cooling liquid. The primary purpose of its utilization as a (3-10) % aqueous emulsion is blade and abrasive treatment of cast iron, carbon steel and steel alloys.Guarantee period of storage – 6 months from the day of manufacture.
Agrinol RGТУ У 23.2-30802090-020-2002Agrinol RG is a working liquid used in the hydraulics of industrial equipment and generally intended for the utilization as a (3-5)% aqueous emulsion in the hydraulics of shaft and mining equipment, including the underground one, at ambient temperature higher than 10°С.Guarantee period of storage – 6 months from the day of manufacture.
Agrinol EHPТУ У 23.2-30802090-025-2004
Agrinol HPТУ У 23.2-30802090-022-2003The technological lubricants Agrinol EHP and Agrinol HP are oil concentrated products which are intended for the utilization as a (2‑5) % emulsion in water with the hardness not higher than 5 mg-equivalent /dm³ on the stage of cold rolling of steel. They can also be utilized as a (5-10)% emulsion in water with the hardness not higher than 17 mg-equivalent/dm³ for the oiling of band steel before wrapping it into a roll with thermal treatment to follow.Both products can be utilized at the treatment of ferrous metals by pressure or cutting. Guarantee period of storage – 6 months from the day of manufacture.Table 102
| Index Name |
Agrinol ET-2U |
Agrinol RG |
Agrinol EHP |
Agrinol HP |
| Appearance |
Homogenous oily dark-brown liquid |
| Smell |
Specific, not irritating |
Acid number, mg КОN/g, not more than |
within 15–23 |
16 |
16 |
12 |
| Kinematic viscosity at 50°С, mm²/s, not more than |
within 20-50 |
100 |
50 |
35 |
Fraction of total mass, %, not more than: |
|
|
|
|
| - mechanical impurities |
0,3 |
0,3 |
– |
– |
| - water |
3 |
5 |
1 |
1 |
| Stability during the storage |
Withstands |
| Density at 20°С, kg/m³ |
880–980 |
900–980 |
880–960 |
920–960 |
| Working emulsion |
| |
10 %- |
3 % |
| Stability, %, not more than, during: |
|
|
|
|
| - 4 h |
0,5 |
0,5 |
– |
– |
| - 6 h |
– |
– |
Withstands |
Withstands |
| pН value, units of рН |
8–10 |
8–10 |
8–9 |
8–9 |
Corrosive influence on metals
|
Withstands |
| Inclination for foam-forming at 20°С, cm³, not more than |
– |
– |
20 |
20 |
| Foam stability at 20°С, сm³, not more than |
– |
– |
10 |
10 |
|